Ethylene-Propylene-Diene-Rubber-Mixture (EPDM)

The thermal behavior of an EPDM rubber mixture was measured between –125°C and 160°C at 10 K/min. The glass transition was detected at –52.5°C. The melting above the glass transition (peak temperature at 31.4°C) is typical for the behavior of a sequence-type EPDM. The further endothermal effects (at 98.6°C and 110°C) are due to the evaporation of processing agents. The presentation in the separate window clearly shows the high sensitivity of the DSC 200 F3 Maia® even for small energetic effects (0.43 J/g).

DSC 200 F3 Maia® - Differential Scanning Calorimeter

This Differential Scanning Calorimeter (DSC) development at NETZSCH unites compactness, robustness and simple operation with high detection sensitivity for your preferred application in material quality control and failure analysis.

DSC 3500 Sirius

DSC 3500 Sirius kompakt yapısı, sağlamlığı, yüksek hassasiyeti ve kolay kullanımı ile gıda, kozmetik, polimer, teknik tekstiller ve organik-inorganik malzeme gibi alanlarda hata analizi ve kalite-güvence için gerekli optimal şartları sunmaktadır.