Polymers — Behavior under Pressure

The extent to which the elastic properties of a seal remain intact after being subjected to a constant load of longer duration is very important. To test this, an elastomer seal was loaded with a force of 3 N and then relieved to 5 mN. Following a 40-hour load time, 21% compression was observed. After a 30-minute relief period, the compression had reversed by 16.2%; after 60 min, by 16.8%. The visco-elastic properties of the elastomer were such that the sample did not return to its original length even after 30 hours. (measurement with TMA 402 F1/F3 Hyperion®)

TMA 402 F1/F3 Hyperion® - Termomekanik Analiz Cihazı

Yeni TMA 402 F1/F3 Hyperion® modelini özel yapan fırınların değiştirilebilir olduğu ve sıcaklığı 150°C ile 1550°C arasında olan  modüler konsepttir, aynı zamanda sistem diğer NETZSCH cihazları ile uyumludur. Fazla sayıda numune tutucu tipi ve ayar olanağı bulunmaktadır. Yeni TMA 402 F1/F3 Hyperion® geniş aralıkta yük ile, yük eklemeden, -3N ile 3N arasında dijital programlanabilir.